RYUDYE-W METAL BINDER GS-50ELF 金粉浆 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
[产品说明] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
金粉专用印花浆。 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
[保存期] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
室温贮藏一年。避免贮存于摄氏40度以上或摄氏低温0度以下。 |
|
|
|
|
|
|
|
|
|
|
|
[环保标准] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
1.符合欧盟对“烷基酚聚氧乙烯醚”(APEO)所定之安全标准(2003/53/EC)号指令;
|
|
2.符合欧盟对“邻苯二甲酸盐(PHTHALATE)”所定之安全标准(2005/84/EC)号指令; |
|
3.符合欧盟禁用有害偶氮染料(AZO)含量不超过30mg/kg (2002/61/EC)号指令; |
|
4.符合欧盟EN71 PART 3对重金属含量的标准; |
|
|
|
|
5.不含PVC(测试方法:FTIR)。 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
[印花处方] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
RYUDYE-W METAL BINDER GS-50ELF |
|
80-70 |
|
|
|
|
金粉 |
|
|
|
20-30 |
|
|
|
|
合计(重量%): |
|
|
100 |
|
|
|
|
|
|
|
|
|
|
|
|
[印花工程] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
印花 → 预热(100℃,1-2分钟)→ 热处理(130-150℃,2-3分钟) |
|
|
|
|
|
|
|
|
|
|
[牢度测试] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
1.洗水牢度测试(60℃×1小时)×4次: 3.5级 |
|
|
|
|
2.摩擦牢度测试JIS标准L-0849(100回/3分钟): 3.0级 |
|
|
|
备注:牢度等级0-5级,其中5级为最好。 |
|
|
|
|
|
|
|
|
|
|
|
|
|
[注意事项] |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
1.请使用600目以下网版。 |
|
|
|
|
|
|
2.不可用氨水调整酸碱值,以免加快金粉变色。 |